| Wiwa: | |
|---|---|
| opoiye: | |

| Awọn ọja Name |
Gbona óò Galvanized GI Irin Coil |
|---|---|
|
Ipele
|
DX51D,SGCC,DX52D,ASTMA653,JISG3302
|
|
Aso Zinc
|
Z40-275g/m²
|
|
Iwọn okun
|
4-5tons
|
|
Epo id
|
508/610mm
|
|
Package
|
Standard Òkun Worthy Package
|
|
MOQ
|
25 toonu
|
|
Spangle
|
Spangle deede,Mini Spangle,Big Spangle
|
|
Iwe-ẹri
|
SGS
|
|
Ohun elo
|
uilding, Orule dì, ailewu odi ati be be lo.
|
|
Akoko Ifijiṣẹ
|
laarin 15-20 ọjọ lẹhin gbigba 30% idogo tabi dale lori Opoiye
|
|
Akoko Isanwo
|
T/T, L/C ti ko le yipada ni oju (30% idogo)
|
|
Iṣowo Akoko
|
EXW, FOB, CFR, CIF
|
Gbona-Dipped Hot-Dipped GI Galvanized Steel Coil jẹ ọja irin ti o ni ipilẹ ti a ṣe apẹrẹ fun awọn ohun elo ile-iṣẹ ti o nilo resistance ipata to lagbara, agbara ẹrọ, ati ibamu ilana. Ti a ṣelọpọ nipasẹ ilana galvanizing ti o gbona-dip, okun yii ṣe ẹya ti a bo zinc ti o nipọn (Z180-Z275g) lori sobusitireti irin-kekere erogba (Q235, SS400 grades), n pese aabo to dara julọ si ọrinrin, itọsi UV, ati awọn idoti oju aye.
Wa ni awọn sisanra lati 0.5mm si 4.0mm ati awọn iwọn to 1500mm, okun ti wa ni iṣapeye fun iṣelọpọ iṣẹ-eru ni ikole, adaṣe, ati awọn ile-iṣẹ ẹrọ. Ilana gbigbona n ṣe idaniloju asopọ irin-irin laarin zinc ati irin, ṣiṣẹda ipele ti o tọ ti o ṣe iwosan ara ẹni awọn irun kekere nipasẹ aabo irubọ.
Aabo Ibaje ti o lagbara :
Z180-Z275 Coating : Apẹrẹ fun ita gbangba / awọn agbegbe ile-iṣẹ (Z180: amayederun ilu, Z275: awọn ohun ọgbin eti okun / kemikali), pẹlu igbesi aye asọtẹlẹ ti awọn ọdun 15-30 da lori itọju (fun apẹẹrẹ, awọn ayewo ọdọọdun).
Idaabobo Ẹbọ : Layer Zinc oxidizes ni pataki si irin, idabobo awọn egbegbe ti a ge ati awọn irẹwẹsi titi ti a fi ṣe atunṣe pẹlu awọ ọlọrọ zinc (fun apẹẹrẹ, Zincalume Paint International).
Awọn ohun-ini Mechanical Ipele Iṣẹ :
Agbara ikore giga (235-400 MPa) ṣe atilẹyin awọn ohun elo igbekalẹ bii awọn opo irin, awọn paati afara, ati awọn fireemu ẹrọ ti o wuwo (fun apẹẹrẹ, awọn gbigbe ẹrọ Caterpillar).
Weldability ti o dara julọ (akoonu erogba kekere ≤0.20%) ati ọna kika, pẹlu awọn oju-ọfẹ spangle ti n mu alurinmorin TIG/MIG kongẹ fun awọn isẹpo to ṣe pataki (fun apẹẹrẹ, awọn asopọ iru ẹrọ ti ita).
Ibamu ilana :
Dara fun elekitiroplating, ti a bo lulú, ati kikun omi, pẹlu iyan chromate pretreatment imudara ifaramọ kun nipasẹ 40% (fun apẹẹrẹ, awọn aṣọ ile-iṣẹ AkzoNobel).
Awọn iwuwo okun nla (awọn toonu 10-20) dinku akoko idinku ni awọn laini iṣelọpọ iyara, pẹlu slitting aṣa ti o wa si awọn iwọn deede (ifarada: +/- 0.5mm fun awọn iwọn 1000mm +).
Ibamu Awọn Iwọn Agbaye :
Pade ASTM A653 (G90), JIS G3302 (SGCC), ati EN 10142 (Z275) awọn ajohunše, aridaju aitasera didara fun awọn rira okeere (fun apẹẹrẹ, UAE awọn iṣẹ amayederun, awọn iṣẹ iwakusa Brazil).
Atunlo 100% ni ipari-aye, pẹlu awọn oṣuwọn imularada zinc ti o kọja 95%, ni ibamu pẹlu awọn ipilẹ eto-ọrọ aje ipin.
Ikole & Amayederun : Awọn ile-iṣelọpọ I-beams, awọn apakan ikanni, ati awọn trusses orule fun awọn ile iṣowo (fun apẹẹrẹ, Imugboroosi Ile Itaja Dubai), awọn afara (fun apẹẹrẹ, San Francisco-Oakland Bay Bridge), ati awọn ohun elo agbara (fun apẹẹrẹ, awọn ohun elo Saudi Aramco).
Automotive & Transportation : Fọọmu awọn paati chassis, awọn fireemu ikoledanu, ati awọn axles tirela fun awọn ọkọ ti o wuwo (fun apẹẹrẹ, awọn oko nla Volvo FH), ti o funni ni aabo lodi si iyọ opopona ati aapọn ẹrọ.
Ẹrọ Iṣẹ : Ti a lo fun awọn fireemu ẹrọ iṣelọpọ, awọn ọna gbigbe, ati awọn tanki ibi ipamọ ni iwakusa (fun apẹẹrẹ, BHP Billiton ore processing), ogbin (fun apẹẹrẹ, awọn olukore John Deere), ati awọn apa iṣelọpọ.
Apa Agbara : Apẹrẹ fun awọn ipilẹ turbine afẹfẹ (fun apẹẹrẹ, awọn oko afẹfẹ Vestas), awọn agbeko ti oorun, ati awọn ẹya agbara ti ita, pẹlu AZ150 alloy alloy (iyan) imudara ooru resistance fun awọn ohun elo oorun.
Q: Bawo ni galvanizing gbona-dip ṣe afiwe si elekitiro-galvanizing?
A: Gbona-dip pese nipọn, awọn ohun elo ti o tọ (30-275g / m²) fun lilo ita gbangba; elekitiro-galvanizing (10-20g/m²) jẹ tinrin ati pe o dara fun awọn ohun elo inu ile ti ohun ọṣọ bi ohun elo aga.
Q: Njẹ a le lo okun yii fun ibi ipamọ omi mimu?
A: Rara, olubasọrọ taara pẹlu omi mimu nilo awọn ohun elo ounjẹ-ounjẹ bi irin alagbara tabi irin-ila epoxy; Irin GI jẹ o dara fun awọn tanki omi ti ko ni agbara ati awọn ọna irigeson.
Q: Kini ọna ti o dara julọ lati yọ iwọn ọlọ ṣaaju kikun?
A: Lo fifẹ abrasive (iyanrin / fifun ibọn) lati ṣaṣeyọri profaili oju-aye Sa2.5, ni idaniloju ifaramọ kikun ti o dara julọ fun agbara igba pipẹ.
Q: Bii o ṣe le rii daju iwuwo ibora lori aaye laisi ibajẹ okun?
A: Lo iwọn sisanra oofa (fun apẹẹrẹ, Fischer XDL) lati wiwọn sisanra ti a bo ti kii ṣe iparun; iye yẹ ki o wa laarin 5% ti awọn pàtó kan ti a bo àdánù.






![]() |
Ẹdọfu Leveler Titọna fifẹ ni lati na ati taara okun irin lati gba apẹrẹ awo to dara julọ. |
Ẹrọ Fun Zinc Lẹhin ti zinc ingot ti wa ni tolera ninu ikoko, awọn sinkii ikoko ti wa ni kikan nipasẹ awọn console ti awọn sinkii ikoko, ati awọn iwọn otutu ti wa ni pa. Ingot zinc ti yo sinu omi zinc. |
![]() |
![]() |
Coiler Okun irin galvanized pẹlu kẹkẹ arbor jẹ ṣeto daradara sinu awọn yipo, deede fun okun jẹ awọn toonu 3-5. |

Onibara idasile
Jẹrisi Bere fun
Ṣiṣejade
Awọn ọja Sowo

Q1: Ṣe o jẹ ile-iṣẹ tabi ile-iṣẹ iṣowo?
A: A jẹ olupese, tọkàntọkàn kaabọ ti o ṣabẹwo si ile-iṣẹ wa.
Q2: Ṣe o le ṣe iṣeduro didara okun okun galvanized rẹ?
A: Didara to dara julọ ni ipilẹ wa ni gbogbo igba. A ni 2 igba didara igbeyewo ṣaaju ki o to ifijiṣẹ.
Iran wa: lati jẹ alamọdaju-kilasi agbaye, ti o gbẹkẹle ati olutaja irin to dayato.
Q3: Kini awọn anfani ti ile-iṣẹ rẹ?
A: Bi o ṣe mọ, iṣowo akọọlẹ wa ni Alibaba.com ati ni Ariwa China jẹ oke 1.
Pupọ ṣe ọpẹ fun igbẹkẹle alabara.
Q4: Kini MOQ rẹ?
A: A ṣe itẹwọgba aṣẹ idanwo rẹ MOQ 25 T lati wa ni sitofudi ni 1 * 20GP.
Opoiye nla le dinku idiyele rẹ.
Q5: Kini ọja akọkọ rẹ?
A: Galvanized, irin coils ti wa ni o kun okeere to Afirca, Southeast Asia, Aringbungbun East, Central
Asia Europe, North & South America ati awọn orilẹ-ede miiran ati agbegbe.